1.3 Stress Intensification Factors
As noted previously, Markl's fatigue tests generated endurance curves for various fitting configurations, such as straight pipe, butt welded pipe, elbows, miters, welding tees, unreinforced and reinforced fabricated tees, mostly using 4" nominal diameter, size-on-size fittings. Markl noticed that the fatigue failures occurred not in the middle of his test spans, but primarily in the vicinity of the fittings, and in those cases, they also occurred at lower stress/cycle combina

Meena Rezkallah, P.Eng.
Mar 29, 20203 min read


1.2.5 Effect of Sustained Loads on Fatigue Strength
In almost all cases the material fatigue curves are generated using a completely alternating stress; i.e., the average stress component is zero. Research has shown that the magnitude of the mean stress can have an effect on the endurance strength of a material, the trend of which is shown below: Note that as the mean stress increases the maximum permissible absolute stress (Sa + Sm) increases, while the permissible alternating stress decreases. The relationship between the al

Meena Rezkallah, P.Eng.
Mar 22, 20202 min read


1.2.4 Cyclic Reduction Factor
At some point, in the vicinity of 7,000 cycles, the (Syc + Syh) limitation intersects the fatigue curve for carbon and low alloy steel. The allowable stress range must therefore be reduced to fit the fatigue curve for cyclic applications with 7,000 cycles or more: SE <= F f (SYC + Syh) Where: f = cyclic reduction factor, as shown in the accompanying table CYCLIC REDUCTION FACTOR (f) | ASME B31.3 Pipe Stress Analysis, Thermal Expansion & Fatigue Design Read More: Introduction

Meena Rezkallah, P.Eng.
Mar 22, 20201 min read


1.2.3 Effect of Fatigue on Piping
A. R. C. Markl investigated the phenomenon of fatigue failure of piping during the 1940's and 1950's, and published his results in papers such as "Piping Flexibility Analysis", published in 1955. He tested a number of configurations (straight pipe, and various fittings, such as pipe elbow, miter bend, unreinforced fabricated tee, welding tee, etc.) by using cyclic displacements to apply alternating bending stresses. Plotting the cycles to failure for each applied displacement

Meena Rezkallah, P.Eng.
Mar 21, 20202 min read


1.2.2 Fatigue Curves
A plot of the cyclic stress capacity of a material is called a fatigue (or endurance) curve. These curves are generated through multiple cyclic tests at different stress levels. The number of cycles to failure usually increases as the applied cyclic stress decreases, often until a threshold stress (known as the endurance limit) is reached below which no fatigue failure occurs, regardless of the number of applied cycles. The endurance limit (for those metals that possess one)

Meena Rezkallah, P.Eng.
Mar 21, 20202 min read